Cast or extruded acrylic: which one belongs in furniture

Cast acrylic is polymerized in a mold, cell by cell. Extruded acrylic is melted and pushed through a die as a continuous sheet. For furniture the difference decides everything: cast material machines and polishes cleanly at furniture thickness, while extruded sheet is thinner, cheaper and prone to crazing at cut edges.

Thick carved cast acrylic slab resting on a pallet on the workshop floor
Cast stock arrives as blocks and thick slabs, not as sheet

What is the actual difference?

It is molecular weight and internal stress. Casting builds long polymer chains slowly in a mold, so the finished block is more uniform and holds together better when a cutter goes through it. Extrusion forces molten material through a die at speed, which aligns the chains and freezes stress into the sheet.

The manufacturer’s own comparison says the same thing in process terms: cell cast sheet is poured as liquid monomer between glass and cured in an autoclave, while extrusion uses grades with a lower molecular weight. Cast material therefore has less tendency to melt or chip during machining, handles long-term mechanical loads better, and comes in far greater thicknesses, over one inch. Extruded sheet is cheaper, holds tighter thickness tolerance and cements faster.

Locked-in stress is invisible until you cut, drill or glue. Then it shows as crazing, the fine white cracks that spread from a hole or an edge. Extruded material also softens at a lower temperature, which is useful if you want to thermoform it and a problem if you want to machine it.

PropertyCast acrylicExtruded acrylic
Made byPolymerizing in a mold or cellMelting and pushing through a die
Thickness availableThin sheet up to solid blocksSheet, generally thinner
MachiningCuts and carves cleanly, chips break awayGums and melts more readily
Crazing risk at cutsLowerHigher, stress relieved cuts are essential
Thickness consistencyVaries slightly across the sheetVery consistent
CostHigherLower
Best forFurniture, sculpture, thick carved partsSignage, glazing, thermoformed shapes

Process, molecular weight, thickness range, machining behavior and cost in the table above follow Polyvantis, “What is the difference between cast and extruded acrylic sheet?” (manufacturer knowledge base, read 18 September 2026). The crazing and joint notes below are what we see on our own shop floor.

End mill cutting the side face of a very thick frosted cast acrylic block
Cast material cuts without gumming, which is what makes deep carving possible

Where does extruded sheet fail in furniture?

Three places, and they are all joints.

  • Bonded seams. Solvent plus locked-in stress equals crazing along the glue line, often weeks after assembly.
  • Fixing holes. A drilled hole concentrates stress. In extruded sheet the cracks start there and radiate.
  • Carved surfaces. A deep texture needs material to cut into. Sheet that is 10mm thick cannot carry a 6mm facet and still be a table.

None of that makes extruded material bad. It is the right choice for a light box or a shop sign. It is the wrong choice for a dining table that has to last a decade.

How do you tell them apart on arrival?

  • Check the masking film. Producers usually print the grade on it, and cast material is labeled as cast or as cell-cast.
  • Drill a test hole in an offcut. Extruded material gums onto the bit sooner and shows a milky ring.
  • Look at the edge of a thick section against the light. Cast stock is generally more even in color through the depth.
  • Ask what thickness range the supplier stocks. A supplier who only holds sheet up to 20mm is not selling you a carved table.

Everything we build starts from cast stock, and we anneal after machining and bonding to take the remaining stress out. You can see the blocks, the routers and the annealing step in the cast acrylic manufacturing process.

Does cast acrylic cost more than it is worth?

For a flat panel, often yes. For anything carved, bonded or thicker than about 20mm, the extra material cost is smaller than the cost of the failures you avoid. A crazed joint is not repairable; it is a replacement.

Related reading: whether cast acrylic furniture turns yellow. Or see the pieces this material becomes in our console and side table range.

Not sure which your drawing needs?

Send it over. We will tell you the thickness the piece actually needs and what it should be cut from.

More cast acrylic guides

  • How thick a cast acrylic table top should be, and what it will weigh

    A solid cast acrylic table top is usually 30mm to 50mm thick for a round table of 1200mm to 1500mm, 40mm to 60mm for a dining table of 1800mm to 2400mm, and 50mm or more beyond that. Low tables run 20mm to 40mm. The span between supports sets the number, not the look.

  • What an acrylic furniture specification should say, line by line

    An acrylic furniture specification should state seven things: the material (virgin cast PMMA), the thickness of every load-bearing part, the surface finish, where the joints go, the base and fixings, the packing, and how the sample and the delivered piece will be checked. Each line closes a gap a factory would otherwise fill with its own cheapest choice.

  • What you are paying for in a piece of solid acrylic furniture

    Solid acrylic furniture is expensive because of weight, waste and hand work. A furniture-grade top is a heavy slab of cast PMMA, carving turns much of that block into chips, and every face is then sanded and polished by hand. Thickness and carving depth move the price far more than the size of the piece.